3D Printing Face shields -> Print quickly and reliably
Hi guys !
First, I hope you are fine and your family too.
I did not post anything since a long time.
I dropped a few 3d printed parts to volunteers assembling face shields for people fighting the coronavirus.
I am pretty amazed how fast the 3d printing community reacted and how big it is becoming.
How to print "quickly and reliably" ?
I put quickly in bracket, because of the speed and the throughput.
Yes for the throughput, speed matters but at what risk: reliability of the print and reliability of the machine.
Safe Slicer settings:
- Larger Extrusion Width (Nozzle: 0.4mm -> 0.5mm, 0.6mm -> 0.72mm, 0.8mm -> 1mm): the geometry of the tip of your nozzle and the geometry of the part to print is the limiting factor.
- Larger Layer Height but not overdo it ( Nozzle: 0.4mm -> 0.28 to 0.32mm, 0.6mm -> 0.4mm): some tuning is needed, the part can become too weak (see cooling/temperature parameters)
- Tune number of perimeters/insets: given the geometry and the extrusion width you can manage to reduce the number of passes made and reduce/avoid the slow shaking movement of the top/bottom or the gap filling (overlap setting is your friend)
- Use Concentric infill for Top/Bottom layers: linear infill or zigzag infill will just take more time
- Cooling parameters: No fan on PETG print for instance, try to reduce it, it makes stronger parts and you can print faster. Set the print time per layer down to 5 or less seconds.
- Keep the same print speed all around, if there is a bit of ringing it does not really matter.
- Keep a safe margin on the extrusion throughput, go to max 75% to 80% of the theoretical limit (https://www.printitindustries.com/pages/print-speed-calculator)
- Print with higher temperature but don't overdo it (retraction can become ineffective after a threshold)
Example printing a single part on PETG at 230C on an Ender 3:
Standard Print Speed 40mm/sec, Retraction speed 25mm/s with 6mm
Layer Height 0.2mm with 0.4mm extrusion width, base line 2h22m
- Same speed with larger extrusion width + cooling settings + concentric top/bottom infill:
0.4mm to 0.5mm with 0.2mm layer height: 1h52m - Same speed with larger layer height (0.5mm extrusion width instead of 0.4mm):
- 0.24mm layer height 1h33m
- 0.28mm 1h22m part good
- 0.32mm 1h12m part correct
- Increasing speed from 40mm/sec to 50mm/sec
- 0.32mm 1h05m (part too weak, start to have under extrusion after short retractions sequences)
- 0.28mm 1h12m part correct
What about reliability ? 2 minor failures only caused by me ^^
Same quality of the prints over and over, print start and you go.
Happy 3D Printing !
Leave 3D Printing Face shields -> Print quickly and reliably to:
Read more #printing3d posts
Best Posts From Julien BOUCARON
We have not curated any of boucaron's posts yet. But you can encourage our curation team to review posts by visiting them regularly and by referring other readers. Because we give priority to frequently read content.
More Posts From Julien BOUCARON
- Gandalf Testing Ender 3 Profile on ChopChop3D Slicer
- ChopChop3D Slicer History in Images
- 3D Printing Face shields -> Print quickly and reliably
- ChopChop3D Slicer BETA forthcoming update
- Platform.io for embedded development
- Tutorial: Setup an Apple MacOS Mojave Virtual Box VM
- Tutorial: How to backup all your Steem posts ?
- High throughput 3D printing with a regular nozzle ^^
- XMas stuff: OpenSCAD Vase/Bowl Generator
- ChopChop3D Slicer BETA_08 is out ! Having fun with the new Brim algorithm